  • Water and the water barrier
  • Where it fails
  • New work
Where to look: the window corner (A), a crack in the open wall (B), the base of the wall (C).

After you tap Send photos

  1. 1

    We confirm they arrived.

    The next page tells you your photos came through.

  2. 2

    A person reads them.

    A person looks at your photos and measurements and writes your price.

  3. 3

    You decide.

    The price is in writing. If it works for you, you pay the deposit and we set the day.

Send photos of the wall

Three shots help most

  • The whole wall
  • The damage, up close
  • A tape measure in the shot

No photos added yet. Up to 4 photos. Large photos are made smaller before sending.

Example: 2 wide by 3 tall

To check that we cover your area

Phone / Email

One is enough. It is where we send your price.

With photos, that is all we ask for a price. Without photos, tick the call box and we call you first.

The wall, layer by layer

Stucco is not waterproof. Some rain always gets behind it. What keeps the wood dry is a layer you never see: the paper and flashing behind the stucco. Here is where it sits, the three places it fails, and what a repair touches.

The layers, outside to inside

outsideinsideabcdef
  • aFinish coat. Color and texture. About 1/8 in.
  • bBrown coat. Makes the wall flat. About 3/8 in.
  • cScratch coat over metal lath. Grips the wall. About 3/8 in.
  • dThe water barrier. Two layers of building paper, with flashing at every opening.
  • eSheathing. Wood panel. It must stay dry.
  • fFraming. Wood studs. It must stay dry.

AAt the window sill

The sealant under the window opens. Water gets in at the corner.

Show the drawing
outsideinsideA123
  1. 1Sealant over a backer rod, between the window and the stucco.
  2. 2Sill flashing. It turns down over the paper below, so water steps out.
  3. 3If the flashing is missing or lapped backwards, water reaches the wood here.

BIn the open wall

A crack takes in more water than the wall can drain.

Show the drawing
outsideinsideB12
  1. 1The crack goes through all three coats.
  2. 2Water runs down the face of the paper. Every fastener is a small hole in it.

CAt the base of the wall

Soil, mulch or new paving covers the exit. Water cannot leave, and the base of the wall stays wet.

Show the drawing
outsideinsideC4 in. min.12
  1. 1Weep screed. The exit at the bottom of the wall.
  2. 2Model code asks for at least 4 in. clear above soil and 2 in. above paving.

RWhat a repair touches

A repair that lasts goes from the finish back to the paper.

  1. 1The stucco is cut back to sound edges, wider than the damage.
  2. 2New paper tucks under the old paper above.
  3. 3And laps over the old paper below, like shingles.
  4. 4New lath laps the old lath. Then scratch, brown and a finish matched to the wall.
  5. 5Sheathing is replaced only where it is wet or soft.
outsideinside14253

General illustration, not a specification. Three-coat stucco on wood framing over a slab. Thicknesses are drawn to one scale, except the paper and flashing, which are drawn thicker than life so the laps can be read. Your wall may be built another way (EIFS, one-coat stucco, stone or brick). Sources: IRC R703.7 and ASTM C926, C1063. Your local code governs.